Polymer Property : Melting Point = 1780 °F Product List

Thermal Properties

Tips: 30 items are displayed at most. For the rest of the results, please contact customer service.
Thermal Properties Metric English Comments
Melting Point 970 - 1000 °C
1780 - 1830 °F
Osprey Metals HTN 2 Brazing Powder
Particle size distribution 1-250 microns.SHAPE: Predominantly spherical PACKAGING: 4 & 20 Kg. Chemical composition and particle size distribution can be adjusted to suit customers' requireme..
Melting Point 970 - 990 °C
1780 - 1810 °F
Wieland 1651 Wilaform Gold
High-quality alloy for all kinds of decoration production.Applications: casting, coin/shape, laminar decoration, pipes, tubingDental
Melting Point 971 - 1088 °C
1780 - 1990 °F
CMW® 100 Copper Alloy
CMW® 100 material is a heat treatable, high strength, high conductivity copper base alloy. Its properties are a combination of highest strength and hardness with relatively high electrical and ther..
Melting Point 971 - 1120 °C
1780 - 2050 °F
Wall Colmonoy COLMONOY® 57 PTA - Nickel-Base Hard-Surfacing Alloy
Description: Colmonoy 57 PTA is a unique Ni-Cr-B alloy containing optimized amounts of precipitated tungsten rich hard phases distributed throughout the matrix. These hard phases offer substantial ..
Melting Point 971 - 1004 °C
1780 - 1839 °F
Williams Advanced Alloys Wambraze™ WB1004 Solder
High-purity vacuum cast materials are manufactured by Williams in a variety of solder alloys, including gold brazing alloys for electronic packaging and high temperature joining vacuum electronic de..