Polymer Property : Melting Point = 1710 °F Product List

Thermal Properties

Tips: 30 items are displayed at most. For the rest of the results, please contact customer service.
Thermal Properties Metric English Comments
Melting Point 930 °C
1710 °F
CLAL-MSX NICLAL 3444 0 Annealed Copper Alloy, Free Cutting Bronze
Main Characteristics: Excellent machineabilityHigh mechanical propertiesSelf lubricating alloyTypical Applications:Parts for connectorsFriction partsBearings-Pinions-Lock pinsInformation provided b..
Melting Point 930 °C
1710 °F
CLAL-MSX NICLAL 3444 H12 1/2 Hard Copper Alloy, Free Cutting Bronze
Main Characteristics: Excellent machineabilityHigh mechanical propertiesSelf lubricating alloyTypical Applications:Parts for connectorsFriction partsBearings-Pinions-Lock pinsInformation provided b..
Melting Point 930 °C
1710 °F
CLAL-MSX NICLAL 3444 H14 4/4 Hard Copper Alloy, diameter < 8 Copper Alloy, Free Cutting Bronze
Main Characteristics: Excellent machineabilityHigh mechanical propertiesSelf lubricating alloyTypical Applications:Parts for connectorsFriction partsBearings-Pinions-Lock pinsInformation provided b..
Melting Point 930 °C
1710 °F
CLAL-MSX NICLAL 3444 H14 4/4 Hard Copper Alloy, diameter > 8 Copper Alloy, Free Cutting Bronze
Main Characteristics: Excellent machineabilityHigh mechanical propertiesSelf lubricating alloyTypical Applications:Parts for connectorsFriction partsBearings-Pinions-Lock pinsInformation provided b..