Thermal Properties | Metric | English | Comments |
---|---|---|---|
Melting Point | 76.7 °C | 170 °F | Peak Melting Temperature; ExxonMobil Method |
ExxonMobil OPTEMA™ TC 130 Molding, extrusion and compounding resin
(discontinued **) OPTEMA TC 130 is an ethylene methyl acrylate copolymer, which can be used in specialty applications such as a carrier for color and additive master batches, a compatibilizer in polymer compounds and.. |