Melting Point 830 - 910 °C
1530 - 1670 °F
Wieland 1007 Wilaform Gold
Silver white gold alloy for all kinds of decoration manufacturing.Applications: casting, chains, coin/shape, laminar decoration, tubingDental
Melting Point 830 - 850 °C
1530 - 1560 °F
Wieland 1408 Wilaform Gold
Hard yellow gold alloy. Easily splintered and polished.Applications: casting, laminar decoration, tubingDental