Thermal Properties | Metric | English | Comments |
---|---|---|---|
Melting Point | 815 °C | 1500 °F | |
Protective Coating PC-Wood Guardian™ Wood Preservative PC-Wood Guardian™ isused in preventing and controlling decay fungi. It is an effective treatment for wood and wood composite to kill and prevent infestations of decay fungi including white and brow.. |
|||
Melting Point | 816 °C | 1500 °F | |
Heatbath/Park Carbo Fluid D Carburizer Organic liquid which is vaporized in a closed furnace to provide a carburizing atmosphere. In some applications it is found to exhibit higher carburization potential than Carbo Fluid HInformation p.. |
|||
Melting Point | 816 °C | 1500 °F | |
Heatbath/Park Carbo Fluid H Carburizer Organic liquid which is vaporized in a closed furnace to provide a carburizing atmosphere. 5-gallon pails or 55-gallon drums.Information provided by Heatbath Corporation - Park Metallurgical. |