Thermal Properties | Metric | English | Comments |
---|---|---|---|
Melting Point | 1495 °C | 2723 °F | |
ATI Allegheny Ludlum AL 403™ Martensitic Stainless Steel Characteristics: corrosion resistant, heat resistant, oxidation resistant up to 1400°F.Information provided by Allegheny Ludlum |