Thermal Properties | Metric | English | Comments |
---|---|---|---|
Melting Point | 49.0 - 59.0 °C | 120 - 138 °F | |
Fine Organics FINALUX G 728 Lubricant Additive Applications: Internal and external lubricant for PVC cables, films, bottles, lead stabilized injection molded articles. Synergistic co-stabilizing properties with Pb-stabilizers.Information provid.. |