Thermal Properties | Metric | English | Comments |
---|---|---|---|
Melting Point | 1356 °C | 2473 °F | |
American Elements Terbium Nanoparticles General DescriptionTerbium (Tb) Nanoparticles, nanodots or nanopowder are black spherical high surface area particles. Nanoscale Terbium Particles are typically 10 - 80 nanometers (nm) with specific.. |