Thermal Properties Metric English Comments
Melting Point 730 °C
1350 °F
Oceanchem Group Calcium Bromide (CaBr2)
Molecular Formula: CaBr2Cas No.: 7789-41-5Use: Calcium Bromide and its formuulated brines are mainly used as completion, workover and packer fluids in oil drilling field.Properties: This product is ..