Thermal Properties | Metric | English | Comments |
---|---|---|---|
Melting Point | 673.9 - 727 °C | 1245 - 1340 °F | |
Lucas-Milhaupt BRAZE 401 Characteristics:Braze 401 is an intermediate temperature filler metal that may be used as a cadmium free substitute for Easy-Flo 30 or used in applications where an intermediate silver-copper-zinc .. |