Thermal Properties Metric English Comments
Melting Point 1260 - 1335 °C
2300 - 2435 °F
Special Metals INCONEL® 718SPF™ Nickel Superalloy, Annealed
Typical annealing - continuous process anneal, 1700°F (927°C) at 15 ft (4.57 m) per minute. This produces ASTM No. 12 grain size. Heat capacity, melting range, moduli, and Poisson's ratio re..
Melting Point 1260 - 1335 °C
2300 - 2435 °F
Special Metals INCONEL® 718SPF™ Nickel Superalloy, Annealed + Aged
Typical annealing - continuous process anneal, 1700°F (927°C) at 15 ft (4.57 m) per minute. This produces ASTM No. 12 grain size. Typical aging - 1750°F (954°C)/1 h/AC plus 1325°F (..