Thermal Properties | Metric | English | Comments |
---|---|---|---|
Melting Point | <= 1235 °C | <= 2255 °F | |
Weartech International WT-190 Cobalt Hardfacing & Wear Resistant Alloy Applications: tri-cone rock bits for oil drillingInformation provided by Weartech International |