Polymer Property : Melting Point = 1165 °F Product List

Thermal Properties

Tips: 30 items are displayed at most. For the rest of the results, please contact customer service.
Thermal Properties Metric English Comments
Melting Point 629.4 - 729.4 °C
1165 - 1345 °F
Lucas-Milhaupt Silvaloy® A34T Brazing Alloy
Silvaloy A34T is used for joining ferrous metals, copper, copper alloys, nickel, nickel alloys and combinations of these metals. The tin content provides good wetting on many difficult wet metals su..