Thermal Properties Metric English Comments
Melting Point 618 - 652 °C
1140 - 1210 °F
Johnson Matthey Matti-sil 56Sn Cadmium Free Brazing Alloy
A very free flowing alloy which is widely used throughout the World for its low melting point and short melting range. Optimum Joint Gap 0.05 - 0.15 mm.AMS 4763AWS A5.8-92 BAg-7BS EN 1044 1999 AG102..
Melting Point 616 °C
1140 °F
Parkway Products Thixomolded® AM60A Magnesium
Thixomolding® is a fabrication technique, similar to injection molding, that uses magnesium alloys as the “resin” instead of plastic. Solid magnesium alloy pellets are fed into the machine, heate..