Melting Point 1082 °C
1980 °F
Materion AlBeMet® AM 162 HIP'd Billet, Annealed
This is a powder metallurgical product produced by gas atomization available as rod, bar, tube and sheet. These shapes are derived by consolidating the Al/Be powder by hot isostatic pressing (HIP) ..