Polymer Property : Melting Point = -81.4 °F Product List

Thermal Properties

Tips: 30 items are displayed at most. For the rest of the results, please contact customer service.
Thermal Properties Metric English Comments
Melting Point -63.0 °C
-81.4 °F
Freezing Point
BASF Ethylene Chlorohydrine
Formula: C2H5ClOCAS: 107-07-3Description: Ethylene chlorohydrine is a colorless liquid, with an alcohol-like odor. It is miscible with water in all proportion.Synonyms: Ethylene chlorhydrin, 2-Chlo..
Melting Point -63.0 °C
-81.4 °F
BASF Dipropylamine
Formula: C6H
Copyright © lookpolymers.com All Rights Reserved