Thermal Properties | Metric | English | Comments |
---|---|---|---|
Melting Point | -68.0 °C | -90.4 °F | |
Dow Corning OS-10 Information provided by Dow Corning |
|||
Melting Point | -68.0 °C | -90.4 °F | |
Dow Corning OS-120 Information provided by Dow Corning |
|||
Melting Point | -68.0 °C | -90.4 °F | |
Dow Corning OS-30 Information provided by Dow Corning |
|||
Melting Point | -68.0 °C | -90.4 °F | |
BASF N-(3-Aminopropyl) imidazole Formula: C6H11N3CAS: 5036-48-6Description: N-(3-Aminopropyl)imidazole is a colorless to yellow liquid, with an amine-like odor. It is miscible with water in all proportions. Synonyms: 1H-Imidazole-.. |