Thermal Properties | Metric | English | Comments |
---|---|---|---|
Melting Point | -135 °C | -211 °F | Freezing Point |
Solvay Chemicals Allyl chloride 3-chloropropene Allyl chloride is mainly used in the manufacture of epichlorohydrin. It is also used in the production of allylic ethers, esters, silanes and quaternary ammonium derivatives.EINECS Number: 203-457-6.. |
|||
Melting Point | -135 °C | -211 °F | Freezing Point |
Solvay Chemicals Allyl chloride High purity – Non stabilized 3-chloropropene Allyl chloride is mainly used in the manufacture of epichlorohydrin. It is also used in the production of allylic ethers, esters, silanes and quaternary ammonium derivatives.EINECS Number: 203-457-6.. |
|||
Melting Point | -135 °C | -211 °F | Freezing Point |
Solvay Chemicals Allyl chloride High purity 3-chloropropene Allyl chloride is mainly used in the manufacture of epichlorohydrin. It is also used in the production of allylic ethers, esters, silanes and quaternary ammonium derivatives.EINECS Number: 203-457-6.. |
|||
Melting Point | -135 °C | -211 °F | Freezing Point |
Chesterton 279 PCS Solvent Cleaner Description: Chesterton® 279 PCS is a state of the art, precision cleaning solvent designed specifically to replace CFC-113, HCFC-141b and other ozone-depleting materials. It is a high effective no.. |