Thermal Properties | Metric | English | Comments |
---|---|---|---|
Melting Point | -112 °C | -170 °F | |
BASF Isobutylvinylether Stabilized 0.1% DEA Formula: C9H12OCAS: 109-53-5Description: Isobutylvinylether is a colorless liquid with an ether-like odor. It is miscible in water.Synonyms: Isobutyl-ethene, 1-Isobutoxyethylene, Isobutyl vinyl eth.. |