Polymer Property : Melting Point = -111.1 °C Product List

Thermal Properties

Tips: 30 items are displayed at most. For the rest of the results, please contact customer service.
Thermal Properties Metric English Comments
Melting Point -111.1 °C
-168.0 °F
at 1.013 bar
Solvay Specialty Polymers Meforex® 143a Ozone-Friendly CFC Replacement
Formula: CH3CF3; Name: 1,1,1 Trifluoroethane. Replaces R 502. Refrigerant blends components for low and middle temperatures.Information provided by Solvay Solexis, Inc.