Thermal Properties | Metric | English | Comments |
---|---|---|---|
Transformation Temperature | 530 °C | 986 °F | |
Ferro IX 2218 Passivation Glasses - High Voltage (Zn-B-Silicates) Typical Powder Form: REG, MVG Zinc-Boro-Silicate passivation glasses are used for hermetic passivation of high voltage diodes, thyristors, and transistors. They provide high junction temperatures a.. |
|||
Transformation Temperature | 530 °C | 986 °F | |
Ferro IX 2443 Passivation Glasses - High Voltage (Zn-B-Silicates) Typical Powder Form: RWG, DSD Zinc-Boro-Silicate passivation glasses are used for hermetic passivation of high voltage diodes, thyristors, and transistors. They provide high junction temperatures a.. |