Thermal Properties | Metric | English | Comments |
---|---|---|---|
Transformation Temperature | 913 °C | 1680 °F | Ac<sub>3</sub> |
Carpenter Pyrotough® 78 Hot Work Die Steel Pyrotough® 78 alloy is a premium quality hot work die steel engineered to withstand the operating temperatures and pressures associated with die casting and hot extrusion operations. The patented c.. |