Thermal Properties Metric English Comments
Transformation Temperature 485 °C
905 °F
Ferro CS 713 Metal Sealing
Glass Type: Si-Ba Alkali Typical Powder Form: VSD Typical Application: Compress.Ferro Metal Sealing glasses are formulated for sealing a wide range of metal packages and parts, including matched se..