Thermal Properties | Metric | English | Comments |
---|---|---|---|
Transformation Temperature | 372 °C | 702 °F | |
Ferro EG 3608 Metal Sealing Glass Type: Si-Ti Alkali Typical Powder Form: VSD Typical Application: Al Ferro Metal Sealing glasses are formulated for sealing a wide range of metal packages and parts, including matched seals fo.. |