Thermal Properties | Metric | English | Comments |
---|---|---|---|
Transformation Temperature | 315 °C | 599 °F | |
Ferro EG 2760 Thick Film Glass Glass Type: Pb-B-Zn Typical Powder Form: MVG, VEG Typical Application: General Ferro produces standard and custom glass products that are used in thick film compositions including resistors, conduc.. |