Polymer Property : Transformation Temperature = 581 °F Product List

Thermal Properties

Tips: 30 items are displayed at most. For the rest of the results, please contact customer service.
Thermal Properties Metric English Comments
Transformation Temperature 305 °C
581 °F
Ferro EG 2018 Display Device
Glass Type: Pb-B (Composite) Typical Powder Form: VEG Typical Application: Seal Ferro's display sealing glasses and dielectrics are low-temperature lead glasses suitable for hermetic sealing and ..
Transformation Temperature 305 °C
581 °F
Ferro EG 2783 Thick Film Glass
Glass Type: Pb-B Typical Powder Form: MVG Typical Application: Die Attachment Ferro produces standard and custom glass products that are used in thick film compositions including resistors, conduct..