Thermal Properties | Metric | English | Comments |
---|---|---|---|
Transformation Temperature | 560 °C | 1040 °F | |
Ferro EG 2807 Metal Sealing Glass Type: Zn-B-Si (devit) Typical Powder Form: VSD Typical Application: Kovar Mo, W Ferro Metal Sealing glasses are formulated for sealing a wide range of metal packages and parts, including matc.. |