Polymer Property : Transformation Temperature = 419 °F Product List

Thermal Properties

Tips: 30 items are displayed at most. For the rest of the results, please contact customer service.
Thermal Properties Metric English Comments
Transformation Temperature 215 °C
419 °F
Martensitic Finish
Latrobe CBS-50â„¢ NiL VIM-VAR High Performance Carburizing Bearing and Gear Steel
CBS-50 NiL VIM-VAR is a carburizing bearing and gear steel designed for service temperatures up to 600°F. The chemistry is engineered such that when suitably carburized and heat treated the case ..