Thermal Properties | Metric | English | Comments |
---|---|---|---|
Transformation Temperature | 91.0 - 99.0 °C | 196 - 210 °F | Expansion Starting Temperature |
Akzo Nobel Expancel® 007 WUF 40 Wet unexpanded microspheres Expancel microspheres are thermoplastic hollow spheres. The microspheres are white spherically formed particles with a thermoplastic shell encapsulating a gas. When the microspheres are heated the.. |