Thermal Properties | Metric | English | Comments |
---|---|---|---|
Transformation Temperature | 191 - 204 °C | 376 - 399 °F | Temp at Max Expansion |
Akzo Nobel Expancel® 930 DU 120 Dry unexpanded microspheres Expancel microspheres are thermoplastic hollow spheres. The microspheres are white spherically formed particles with a thermoplastic shell encapsulating a gas. When the microspheres are heated the.. |