Thermal Properties | Metric | English | Comments |
---|---|---|---|
Transformation Temperature | -8.00 °C | 17.6 °F | TR10; ASTM D1329 |
3M Dyneon™ FLS 2530 Fluoroelastomer 3M™ Dyneon™ Fluoroelastomer FLS 2530 can be compounded using standard water cooled internal mixers or two-roll mills with standard fillers and ingredients utilized in typical fluoroelastomer formu.. |