Polymer Property : Transformation Temperature = 160 °F Product List

Thermal Properties

Tips: 30 items are displayed at most. For the rest of the results, please contact customer service.
Thermal Properties Metric English Comments
Transformation Temperature 71.0 - 81.0 °C
160 - 178 °F
Expansion Starting Temperature
Akzo Nobel Expancel® 820 SL 80 Unexpanded microspheres in aqueous dispersion
Expancel microspheres are thermoplastic hollow spheres. The microspheres are white spherically formed particles with a thermoplastic shell encapsulating a gas. When the microspheres are heated the..