Thermal Properties Metric English Comments
Transformation Temperature 122 - 132 °C
252 - 270 °F
Expansion Starting Temperature
Akzo Nobel Expancel® 930 DU 120 Dry unexpanded microspheres
Expancel microspheres are thermoplastic hollow spheres. The microspheres are white spherically formed particles with a thermoplastic shell encapsulating a gas. When the microspheres are heated the..
Transformation Temperature 122 - 132 °C
252 - 270 °F
Expansion Starting Temperature
Akzo Nobel Expancel® 092 DU 120 Dry unexpanded microspheres
Expancel microspheres are thermoplastic hollow spheres. The microspheres are white spherically formed particles with a thermoplastic shell encapsulating a gas. When the microspheres are heated the..