Thermal Properties | Metric | English | Comments |
---|---|---|---|
Transformation Temperature | -27.8 - -17.2 °C | -18.0 - 1.00 °F | Average value: -22.0 °C Grade Count:3 |
Overview of materials for Thermoplastic Polyurethane, Elastomer, Polyester Grade This property data is a summary of similar materials in the MatWeb database for the category "Thermoplastic Polyurethane, Elastomer, Polyester Grade". Each property range of values reported is minim.. |