Songhan Plastic Technology Co.,Ltd.
 POLYMER SEARCH

Polymer Property : Transformation Temperature = -2.00 °C Product List

Thermal Properties

Tips: 30 items are displayed at most. For the rest of the results, please contact customer service.
Thermal Properties Metric English Comments
Transformation Temperature -2.00 °C
28.4 °F
TR 10
3M Dyneon™ PFE 133TBZ High Temperature Perfluoroelastomer
3M™ Dyneon™ PFE 133TBZ is a technically advanced high temperature perfluorelastomer (HT PFE). It is designed to meet the challenges of higher temperature plasma applications. It is classified as F..
Transformation Temperature -2.00 °C
28.4 °F
TR10
3M Dyneon™ 131TZ High Temperature Perfluoroelastomer
3M™ Dyneon™ 131TZ is a technically advanced high temperature perfluoroelastomer (HT PFE). It is designed to meet the challenges of higher temperature applications. It is classified as FFKM per AST..
Transformation Temperature -2.00 °C
28.4 °F
TR10
3M Dyneon™ 81TZ High Temperature Perfluoroelastomer
3M™ Dyneon™ PFE 81TZ is a technically advanced high temperature perfluoroelastomer (HT PFE). It is designed to meet the challenges of higher temperature applications. It is classified as FFKM per ..
Transformation Temperature -2.00 °C
28.4 °F
TR10
3M Dyneon™ PFE 4131TZ High Temperature Perfluoroelastomer
3M™ Dyneon™ PFE 4131TZ is an incorporated cure high temperature perfluoroelastomer (HT PFE). It is designed to meet the challenges of higher temperature applications. It is classified as FFKM per ..
Transformation Temperature -2.00 °C
28.4 °F
TR10
3M Dyneon™ PFE 60Z Perfluoroelastomer
Dyneon™ PFE 60 Z is a technically advanced peroxide curable perfluoroelastomer, designed to meet the challenges of demanding sealing applications. It’s fully fluorinated back bone structure provid..
Transformation Temperature -2.00 °C
28.4 °F
TR10
3M Dyneon™ PFE 80Z Peroxide Cure Perfluoroelastomer
3M™ Dyneon™ Peroxide Cure Perfluoroelastomer PFE 80Z is a technically advanced peroxide curable perfluoroelastomer. This product is designed to have improved acid resistance and lower metal ion ex..
Transformation Temperature -2.00 °C
28.4 °F
TR10
3M Dyneon™ TFE 90Z Peroxide Cure Perfluoroelastomer
3M™ Dyneon™ Peroxide Cure Perfluoroelastomer PFE 90Z is a technically advanced peroxide curable perfluoroelastomer, designed to meet the challenges of demanding sealing applications. It is classif..
Transformation Temperature -2.00 °C
28.4 °F
TR 10
3M Dyneon™ PFE 132TBZ High Temperature Perfluoroelastomer
3M™ Dyneon™ PFE 132TBZ is a technically advanced high temperature perfluorelastomer (HT PFE). It is designed to meet the challenges of higher temperature plasma applications. It is classified as F..
Transformation Temperature -2.00 °C
28.4 °F
TR 10
3M Dyneon™ PFE 191TZ High Temperature Perfluoroelastomer
3M™ Dyneon™ PFE 81TZ, PFE 131TZ and PFE 191TZ are technically advanced high temperature perfluorelastomers (HT PFE). They are designed to meet the challenges of higher temperature applications. Th..
Copyright © lookpolymers.com All Rights Reserved