Thermal Properties Metric English Comments
Ring & Ball Softening Point >= 55.0 °C
>= 131 °F
Lucobit Lucobit® 1210A Ethylene Copolymer Bitumen
Lucobit 1210A is a mixture of ethylene copolymers and special bitumen. Addition of Lucobit to bitumen increases its viscosity and broadens the range of plasticity.Lucobit 1210A in asphalt mixtures ..
Ring & Ball Softening Point >= 55.0 °C
>= 131 °F
Lucobit Lucolast® 7010 Ethylene Butyl Acrylate Asphalt Additive
Lucolast® 7010 is a polar copolymer consisting of ethylene and butyl acrylate with low crystallinity. Addition of Lucolast 7010 to bitumen increases its viscosity, broadens the range of plasticit..
Ring & Ball Softening Point 55.0 - 190 °C
131 - 374 °F
Average value: 107 °C Grade Count:5
Overview of materials for Ethylene Butyl Acrylate
This property data is a summary of similar materials in the MatWeb database for the category "Ethylene Butyl Acrylate". Each property range of values reported is minimum and maximum values of approp..