Thermal Properties Metric English Comments
Ring & Ball Softening Point 161 - 179 °C
322 - 354 °F
Average value: 170 °C Grade Count:3
Overview of materials for Thermoplastic Polyurethane, Elastomer, Polyester Grade
This property data is a summary of similar materials in the MatWeb database for the category "Thermoplastic Polyurethane, Elastomer, Polyester Grade". Each property range of values reported is minim..
Ring & Ball Softening Point 161 °C
322 °F
ASTM E28-92
Lubrizol ESTANE® 5701 Ester Based Thermoplastic Polyurethane
Features: Displays Low Temperature Flexibility and Abrasion Resistance.Uses: Audio Tape Binder and Screen Printing Inks, Inks and Lacquers, Cast Film for LaminationAvailable in Americas and AsiaInfo..