Songhan Plastic Technology Co.,Ltd.
 POLYMER SEARCH

Polymer Property : Ring & Ball Softening Point = 271 °F Product List

Thermal Properties

Tips: 30 items are displayed at most. For the rest of the results, please contact customer service.
Thermal Properties Metric English Comments
Ring & Ball Softening Point 133 °C
271 °F
ASTM E28
Westlake Epolene® C-17 Coating Grade - Highly Branched Medium Molecular Weight Polyethylene Polymer
Product Description: Epolene C-17 is a branched low density polyethylene with a relatively high melt point and viscosity compared to other Epolene C-type Polymers. It is useful to modify paraffin wa..
Ring & Ball Softening Point 133 °C
271 °F
ASTM E28
Westlake Epolene® C-17P Coating Grade - Branched Medium Molecular Weight Polyethylene Polymer
Description: Epolene C-17P is a branched low density polyethylene powder with a relatively high melt point and viscosity compared to other Epolene C-type Polymers. It is useful to modify paraffin wa..
Copyright © lookpolymers.com All Rights Reserved