Thermal Properties Metric English Comments
Ring & Ball Softening Point >= 125 °C
>= 257 °F
IEC 60335-1
Styron CALIBREâ„¢ 7100-15 Polycarbonate
CALIBREâ„¢ 7100-15 glass-reinforced resin offers increased modulus and improved heat distortion resistance, with minimal shrinkage. It also offers outstanding UL-94 flammability ratings. CALIBR..
Ring & Ball Softening Point >= 125 °C
>= 257 °F
IEC 60335-1
Styron CALIBREâ„¢ 7100-8 Polycarbonate
CALIBREâ„¢ 7100-8 glass-reinforced resin offers increased modulus and improved heat distortion resistance, with minimal shrinkage. It also offers outstanding UL-94 flammability ratings. CALIBRE..
Ring & Ball Softening Point >= 125 °C
>= 257 °F
IEC 60335-1
Styron CALIBREâ„¢ 7101-15 Polycarbonate
CALIBREâ„¢ 7101-15 glass-reinforced resin offers increased modulus and improved heat distortion resistance, with minimal shrinkage. It also offers outstanding UL-94 flammability ratings. CALIBR..
Ring & Ball Softening Point >= 125 °C
>= 257 °F
IEC 60335-1
Styron CALIBREâ„¢ 7101-8 Polycarbonate
CALIBREâ„¢ 7101-8 glass-reinforced resin offers increased modulus and improved heat distortion resistance, with minimal shrinkage. It also offers outstanding UL-94 flammability ratings. CALIBRE..
Ring & Ball Softening Point >= 125 °C
>= 257 °F
IEC 60335-1
Styron CALIBREâ„¢ 7102-15 Polycarbonate
CALIBREâ„¢ 7102-15 glass-reinforced resin offers increased modulus and improved heat distortion resistance, with minimal shrinkage. It also offers outstanding UL-94 flammability ratings. CALIBR..
Ring & Ball Softening Point >= 125 °C
>= 257 °F
IEC 60335-1
Styron CALIBREâ„¢ 7102-8 Polycarbonate
CALIBREâ„¢ 7102-8 glass-reinforced resin offers increased modulus and improved heat distortion resistance, with minimal shrinkage. It also offers outstanding UL-94 flammability ratings. CALIBRE..
Ring & Ball Softening Point >= 125 °C
>= 257 °F
IEC 60335-1
Styron CALIBREâ„¢ 7103-15 Polycarbonate
CALIBREâ„¢ 7103-15 glass-reinforced resin offers increased modulus and improved heat distortion resistance, with minimal shrinkage. It also offers outstanding UL-94 flammability ratings. CALIBR..
Ring & Ball Softening Point >= 125 °C
>= 257 °F
IEC 60335-1
Styron CALIBREâ„¢ 7103-8 Polycarbonate
CALIBREâ„¢ 7103-8 glass-reinforced resin offers increased modulus and improved heat distortion resistance, with minimal shrinkage. It also offers outstanding UL-94 flammability ratings. CALIBRE..
Ring & Ball Softening Point >= 125 °C
>= 257 °F
IEC 60335-1
Styron CALIBREâ„¢ 7104-8 Polycarbonate
CALIBREâ„¢ 7104-8 glass-reinforced resin offers increased modulus and improved heat distortion resistance, with minimal shrinkage. It also offers outstanding UL-94 flammability ratings. CALIBRE..