Thermal Properties Metric English Comments
Ring & Ball Softening Point 112 - 145 °C
234 - 293 °F
Average value: 130 °C Grade Count:4
Overview of materials for EMAAA Terpolymer
This property data is a summary of similar materials in the MatWeb database for the category "EMAAA Terpolymer". Each property range of values reported is minimum and maximum values of appropriate M..
Ring & Ball Softening Point 112 °C
234 °F
ASTM E28
Arkema Group LOTADER® 8200 Terpolymer Ethylene - Acrylic Ester - Maleic Anhydride
LOTADER 8200 is a random terpolymer of Ethylene, Acrylic Ester and Maleic Anhydride, polymerized under high pressure in an autoclave process. Due to its properties (reactivity, fluidity), LOTADER 82..