Thermal Properties | Metric | English | Comments |
---|---|---|---|
Ring & Ball Softening Point | 96.0 °C | 205 °F | ASTM E28-99 |
3M Scotch-Weld™ 3762LM Low Melt Adhesive Excellent “hot-tack”, fast setting for corrugated, beadboard, recouperage, repacking chipboard, wood; Economical, general purpose and Use with low melt applicator onlyInformation provided by 3M |