Thermal Properties | Metric | English | Comments |
---|---|---|---|
Ring & Ball Softening Point | 93.0 °C | 199 °F | ASTM E28-99 |
3M Scotch-Weld™ 6116 Bulk only Adhesive Same as 6111 but Lower than normal viscosity and mainly used on fabrics.Information provided by 3M |
|||
Ring & Ball Softening Point | 93.0 °C | 199 °F | ASTM E28-99 |
3M Scotch-Weld™ 3750 Tan Hot Melt Adhesive Low viscosity for high flow rate, increased production and Good hot tack, quick grab for packaging and woodworkingInformation provided by 3M |