Thermal Properties | Metric | English | Comments |
---|---|---|---|
Ring & Ball Softening Point | 91.0 °C | 196 °F | ASTM E28 |
DuPont Elvax® 4320 Ethylene Vinyl Acetate
(discontinued **) DuPont™ Elvax® 4320 is an ethylene-vinyl acetate / acid terpolymer resin for use in industrial applications.ApplicationsElvax® 4320 resins can be used for the following applications: adhesives, s.. |