Polymer Property : Ring & Ball Softening Point = 176 °F Product List

Thermal Properties

Tips: 30 items are displayed at most. For the rest of the results, please contact customer service.
Thermal Properties Metric English Comments
Ring & Ball Softening Point 80.0 °C
176 °F
ASTM E28
DuPont Elvax® 205W Ethylene Vinyl Acetate  (discontinued **)
DuPont™ Elvax® 205W is an ethylene-vinyl acetate copolymer resin containing an anti-blocking additive for use in industrial applications. This resin is supplied in pellet form and to prevent the p..