Polymer Property : Ring & Ball Softening Point = 174 °C Product List

Thermal Properties

Tips: 30 items are displayed at most. For the rest of the results, please contact customer service.
Thermal Properties Metric English Comments
Ring & Ball Softening Point 174 °C
345 °F
ASTM E-28-92
Lubrizol ESTANE® 5714 Ether Based Thermoplastic Polyurethane
Features: Low Temperature Flexibility, Excellent Abrasion, Fungal, and Chemical Resistance, and Hydrolytic Stability. Adhesives can be applied from solution or extruded as a melt coating. The resin ..