Thermal Properties | Metric | English | Comments |
---|---|---|---|
Ring & Ball Softening Point | 153 °C | 307 °F | |
Arkema Group OREVAC® 9304 EVA Terpolymer OREVAC® is a range of ethylene-vinyl acetate copolymers modified by adjunction of polar groups which, when molten, have excellent adhesive properties to various substrates. They are supplied as fre.. |