Thermal Properties | Metric | English | Comments |
---|---|---|---|
Ring & Ball Softening Point | 140 °C | 284 °F | ASTM E28-99 |
3M Scotch-Weld™ 6111 Green Bulk only Adhesive Same as 6111 tan but green in colorInformation provided by 3M |
|||
Ring & Ball Softening Point | 140 °C | 284 °F | ASTM E28-99 |
3M Scotch-Weld™ 6111 Tan Bulk only Adhesive Sprayable 100% solventless adhesive for most foams, fabrics, plastics, particle board and thin metalInformation provided by 3M |