Clash Berg Stiffness Temperature -17.0 °C
1.40 °F
T-10000 Torsional stiffness ASTM D1043-72(1981)
DuPont Performance Polymers Hypalon® 4085 Chlorosulfonated Polyethylene Rubber, Carbon Black Filled Compound  
Carbon black compound with 100 parts Hypalon; 27.8 parts sublimed litharge dispersion; 55 parts carbon black; 55 parts aromatic process oil; 0.5 parts MTBS; and 2 parts Tetrone® A rubber accelerato..
Clash Berg Stiffness Temperature -17.0 °C
1.40 °F
T-10000 Torsional stiffness ASTM D1043-72(1981)
DuPont Performance Polymers Hypalon® 45 Chlorosulfonated Polyethylene Rubber, Mineral Filled Compound  (discon
Mineral filled compound with 100 parts Hypalon; 80 parts hard clay; 4 parts magnesia; 30 parts aromatic process oil; 3 parts pentaerythritol; and 2 parts Tetrone® A rubber accelerator (from DuPont ..