Polymer Property : Clash Berg Stiffness Temperature = -9.40 °F Product List

Thermal Properties

Tips: 30 items are displayed at most. For the rest of the results, please contact customer service.
Thermal Properties Metric English Comments
Clash Berg Stiffness Temperature -23.0 °C
-9.40 °F
T-10000 Torsional stiffness ASTM D1043-72(1981)
DuPont Performance Polymers Hypalon® 20 Chlorosulfonated Polyethylene Rubber, Carbon Black Filled Compound  (d
Carbon black compound with 100 parts Hypalon; 27.8 parts sublimed litharge dispersion; 55 parts carbon black; 55 parts aromatic process oil; 0.5 parts MTBS; and 2 parts Tetrone® A rubber accelerato..