Thermal Properties | Metric | English | Comments |
---|---|---|---|
Clash Berg Stiffness Temperature | -61.1 °C | -78.0 °F | At 10,000 psi (69 Mpa); ASTM D1043 |
Advanced Polymer Alloys Alcryn® 2250 UT Melt Processable Rubber Alcryn melt-processable rubber (MPR) is a true rubber, based on a partially cross-linked, chlorinated olefin interpolymer alloy. Alcryn is designed for the manufacture of rubber parts with high prod.. |